Analysis of mechanical properties of B fibres by means of fractographical analysis of their fracture surfaces

  1. TitleAnalysis of mechanical properties of B fibres by means of fractographical analysis of their fracture surfaces
    Author Iždinský Karol 1959-    SCOPUS    RID
    Co-authors Jerz Jaroslav 1965-    SCOPUS    RID    ORCID

    Romančík Viktor

    Ivan Jozef 1936-

    Issue dataBratislava : ÚMMS SAV , 1993. - s. 25-26
    Languageeng - English
    CountryCS - Czechoslovakia
    Document kindrozpis článkov z periodík (rzb)
    UDC669.018.9
    Keywordsbórové vlákna * fraktografiská analýza * Weibullova distribúcia * strojárstvo všeobecné
    Year1993