Number of the records: 1  

Micro and nano-indentation of MoSi2

  1. TitleMicro and nano-indentation of MoSi2
    Author Henžel Miroslav SAVMATVY - Ústav materiálového výskumu SAV
    Co-authors Kovalčík Jozef SAVMATVY - Ústav materiálového výskumu SAV

    Dusza Ján 1952 SAVMATVY - Ústav materiálového výskumu SAV    SCOPUS    SCOPUS

    Juhász A.

    Lendvai J.

    Source document Journal of Materials Science. Vol. 39, no. 11 (2004), p. 3769-3772
    Languageeng - English
    CountryGB - Great Britian
    Document kindrozpis článkov z periodík (rbx)
    CitationsRAU, J. V. - TEGHIL, R. - FERRO, D. - GENEROSI, A. - ALBERTINI, V. Rossi - SPOLITI, M. - BARINOV, S. M. Deposition and characterisation of MoSi2 films. In THIN SOLID FILMS, 2010, vol.518, no.8, 2050-2055.
    FANG, SQ., HUANG, QH., QIAO, YJ., WANG, JH., JIA, Q.: 2009 Heat Treatment of Metals, vol. 34, no. 8, p. 7-10
    PENG, Qiong - LI, Jin - HE, Chaoyu - TANG, Chao - ZHONG, Jianxin. First-principles study of magnetic properties of ultra-thin MoSi2 films. In JOURNAL OF APPLIED PHYSICS. ISSN 0021-8979, 2018, vol. 123, no. 10, pp.
    GIANCHANDANI, Pardeep Kumar - CASALEGNO, Valentina - SALVO, Milena - FERRARIS, Monica - DLOUHY, Ivo. "Refractory Metal, RM Wrap": A tailorable, pressure-less joining technology. In CERAMICS INTERNATIONAL. ISSN 0272-8842, 2019, vol. 45, no. 4, pp. 4824-4834.
    PELLEG, Joshua. Deformation in Nano Silicides. In Engineering Materials, 2019-01-01, pp. 155-162. ISSN 16121317. Dostupné na: https://doi.org/10.1007/978-3-030-22598-8_9.
    CategoryADCA - Scientific papers in foreign journals registered in Current Contents Connect with IF (impacted)
    Category of document (from 2022)V3 - Vedecký výstup publikačnej činnosti z časopisu
    Type of documentčlánok
    Year2004
    Registered inWOS
    Registered inSCOPUS
    Registered inCCC
    DOI 10.1023/B:JMSC.0000030734.94136.ed
    article

    article

    rokCCIFIF Q (best)JCR Av Jour IF PercSJRSJR Q (best)CiteScore
    A
    rok vydaniarok metrikyIFIF Q (best)SJRSJR Q (best)
    200420030.826
Number of the records: 1  

  This site uses cookies to make them easier to browse. Learn more about how we use cookies.