Investigation of thermal properties of the Ge-As-Se glasses by differential scanning calorimetry with heat flow harmonic modulation

  1. TitleInvestigation of thermal properties of the Ge-As-Se glasses by differential scanning calorimetry with heat flow harmonic modulation
    Author Bilanych V.S.
    Co-authors Onyshchak V.B.

    Rizak I.M.

    Csach Kornel 1953-2023 SAVEXFYZ - Ústav experimentálnej fyziky SAV

    Flachbart Karol 1952 SAVEXFYZ - Ústav experimentálnej fyziky SAV    SCOPUS    RID    ORCID

    Rizak V.M.

    Source document Journal of Non-Crystalline Solids. Vol. 366, no. 1 (2013), p. 48-53
    Languageeng - English
    Document kindrozpis článkov z periodík (rbx)
    CitationsSRIVASTAVA, Archana - TIWARI, S. N. - UPADHYAY, A. N. - ZULFEQUAR, M. - KHAN, Shamshad A. First-order phase transformation and structural studies in Se85In15-xZnx chalcogenide glasses. In JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY. ISSN 1388-6150, 2017, vol. 129, no. 3, pp. 1435-1444.
    AHMADPOUR, S. - REZVANI, M. - BAVAFA, P. The effect of Sn on the physical and optical properties of (Se0.6As0.1Ge0.3)(100-x)Sn-x glasses. In SPECTROCHIMICA ACTA PART A-MOLECULAR AND BIOMOLECULAR SPECTROSCOPY. ISSN 1386-1425, 2018, vol. 205, pp. 258-263.
    MISHRA, Surabhi - LOHIA, Pooja - DWIVEDI, D. K. Structural and optical properties of (Ge-11.5 Se-67.5 Te-12.5)(100-x) Sb-x (0 <= x <= 30) chalcogenide glasses: A material for IR devices. In INFRARED PHYSICS & TECHNOLOGY. ISSN 1350-4495, 2019, vol. 100, pp. 109-116.
    CategoryADCA - Scientific papers in foreign journals registered in Current Contents Connect with IF (impacted)
    Category of document (from 2022)V3 - Vedecký výstup publikačnej činnosti z časopisu
    Type of documentčlánok
    Year2013
    Registered inWOS
    Registered inSCOPUS
    Registered inCCC
    DOI 10.1016/j.jnoncrysol.2012.11.045
    article

    article

    rokCCIFIF Q (best)JCR Av Jour IF PercSJRSJR Q (best)CiteScore
    A
    rok vydaniarok metrikyIFIF Q (best)SJRSJR Q (best)
    201320121.597Q10.755Q1
Number of the records: 1  

  This site uses cookies to make them easier to browse. Learn more about how we use cookies.