Study of high-temperature interaction of the superalloys with molten fluorides

  1. NázovStudy of high-temperature interaction of the superalloys with molten fluorides
    Autor Patel Niketan Sarabhai 1985 SAVANOCH - Ústav anorganickej chémie SAV
    Spoluautori Pavlík Viliam 1978 SAVANOCH - Ústav anorganickej chémie SAV    ORCID

    Kubíková Blanka 1977 SAVANOCH - Ústav anorganickej chémie SAV    ORCID

    Nosko Martin SAVMAMES - Ústav materiálov a mechaniky strojov SAV    SCOPUS    ORCID

    Danielik Vladimír

    Boča Miroslav 1973 SAVANOCH - Ústav anorganickej chémie SAV    SCOPUS    RID    ORCID

    Zdroj.dok. HTMC XVI. 16th IUPAC high temperature materials chemistry conference, july 2 - 6, 2018, Ekaterinburg, Russia : book of abstracts. P. 175. - Ekaterinburg, Russia : Ural State Pedagogical University, 2018 ; HTMC XVI. IUPAC Conference on High Temperature Materials Chemistry
    Jazyk dok.eng - angličtina
    KrajinaRU - Ruská federácia
    Druh dok.rozpis článkov z periodík (rzb)
    KategóriaAFG - Abstrakty príspevkov zo zahraničných konferencií
    Rok vykazovania2018
    článok

    článok

    rok vydaniarok metrikyIFIF Q (best)SJRSJR Q (best)
    2018
Počet záznamov: 1  

  Tieto stránky využívajú súbory cookies, ktoré uľahčujú ich prezeranie. Ďalšie informácie o tom ako používame cookies.