Počet záznamov: 1  

Correlation between strain-rate sensitivity and viscous properties derived from dynamic nanoindentation of ultrafine-grained Al-Zn alloys

  1. NázovCorrelation between strain-rate sensitivity and viscous properties derived from dynamic nanoindentation of ultrafine-grained Al-Zn alloys
    Autor Chinh Nguyen Quang
    Spoluautori Csanádi Tamás SAVMATVY - Ústav materiálového výskumu SAV    SCOPUS    ORCID

    Gubicza Jenö

    Valiev R.Z.

    Zdroj.dok. MRS Communications. Vol. 9, no. 1 (2019), p. 310-314
    Jazyk dok.eng - angličtina
    KrajinaGB - Veľká Británia
    Druh dok.rozpis článkov z periodík (rbx)
    OhlasyCHEN, C. - YU, J.J. - LU, J.Y. - ZHANG, J. - SU, X. - QIAN, C.H. - CHEN, Y.L. - JI, W.X. - LIU, M.P. Phase Transformation in Al/Zn Multilayers during Mechanical Alloying. In ACTA METALLURGICA SINICA-ENGLISH LETTERS. ISSN 1006-7191, OCT 2023, vol. 36, no. 10, p. 1709-1718. Dostupné na: https://doi.org/10.1007/s40195-023-01586-9.
    KategóriaADCA - Vedecké práce v zahraničných karentovaných časopisoch impaktovaných
    Kategória (od 2022)V3 - Vedecký výstup publikačnej činnosti z časopisu
    Typ výstupučlánok
    Rok vykazovania2019
    Registrované vWOS
    Registrované vSCOPUS
    Registrované vCCC
    DOI 10.1557/mrc.2018.226
    článok

    článok

    rokCCIFIF Q (best)JCR Av Jour IF PercSJRSJR Q (best)CiteScore
    A
    rok vydaniarok metrikyIFIF Q (best)SJRSJR Q (best)
    201920181.935Q31.050Q1
Počet záznamov: 1  

  Tieto stránky využívajú súbory cookies, ktoré uľahčujú ich prezeranie. Ďalšie informácie o tom ako používame cookies.