Doping efficiency and electron transport in Al-doped ZnO films grown by atomic layer deposition

  1. NázovDoping efficiency and electron transport in Al-doped ZnO films grown by atomic layer deposition
    Autor Mošková Antónia 1958 SAVELEK - Elektrotechnický ústav SAV
    Spoluautori Moško Martin 1958 SAVELEK - Elektrotechnický ústav SAV    ORCID

    Precner Marián 1987 SAVELEK - Elektrotechnický ústav SAV    ORCID

    Mikolášek M.

    Rosová Alica 1962 SAVELEK - Elektrotechnický ústav SAV    ORCID

    Mičušík Matej 1977- SAVPOLYM - Ústav polymérov SAV    ORCID

    Štrbík Vladimír 1954 SAVELEK - Elektrotechnický ústav SAV

    Šoltýs Ján 1977 SAVELEK - Elektrotechnický ústav SAV    ORCID

    Gucmann Filip 1987 SAVELEK - Elektrotechnický ústav SAV    ORCID

    Dobročka Edmund 1955 SAVELEK - Elektrotechnický ústav SAV    ORCID

    Fröhlich Karol 1954 SAVELEK ; SAVCEMEA - Elektrotechnický ústav SAV    ORCID

    Zdroj.dok. Journal of Applied Physics. Vol. 130 (2021), no. 035106
    Jazyk dok.eng - angličtina
    Druh dok.rozpis článkov z periodík (rbx)
    OhlasyFEDOROV, F.S. - SIMONENKO, N.P. - ARSENOV, P.V. - ZAYTSEV, V. - SIMONENKO, T.L. - GOIKHMAN, B.V. - VOLKOV, I.A. - SIMONENKO, E.P. - NASIBULIN, A.G. Study of programmed co-precipitation of aluminum doped zinc oxide for high precision design of gas analytical units. In APPLIED SURFACE SCIENCE. ISSN 0169-4332, DEC 30 2022, vol. 606. Dostupné na: https://doi.org/10.1016/j.apsusc.2022.154717.
    GOIKHMAN, B.V. - FEDOROV, F.S. - SIMONENKO, N.P. - SIMONENKO, T.L. - FISENKO, N.A. - DUBININA, T.S. - OVCHINNIKOV, G. - LANTSBERG, A.V. - LIPATOV, A. - SIMONENKO, E.P. - NASIBULIN, A.G. Quantum of selectivity testing: detection of isomers and close homologs using an AZO based e-nose without a prior training. In JOURNAL OF MATERIALS CHEMISTRY A. ISSN 2050-7488, APR 12 2022, vol. 10, no. 15, p. 8413-8423. Dostupné na: https://doi.org/10.1039/d1ta10589b.
    SINGH, R. - MUKHERJEE, S.K. Correlation of structural, electrical and optical properties of Al-doped ZnO TCOs. In JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS. ISSN 0957-4522, MAR 2022, vol. 33, no. 9, p. 6969-6980. Dostupné na: https://doi.org/10.1007/s10854-022-07876-9.
    ZHAO, K. - XIE, J.Y. - ZHAO, Y.D. - HAN, D.D. - WANG, Y. - LIU, B. - DONG, J.C. Investigation on Transparent, Conductive ZnO:Al Films Deposited by Atomic Layer Deposition Process. In NANOMATERIALS. JAN 2022, vol. 12, no. 1. Dostupné na: https://doi.org/10.3390/nano12010172.
    KategóriaADCA - Vedecké práce v zahraničných karentovaných časopisoch impaktovaných
    Kategória (od 2022)V3 - Vedecký výstup publikačnej činnosti z časopisu
    Typ výstupučlánok
    Rok vykazovania2021
    Registrované vWOS
    Registrované vSCOPUS
    Registrované vCCC
    DOI 10.1063/5.0053757
    článok

    článok

    rokCCIFIF Q (best)JCR Av Jour IF PercSJRSJR Q (best)CiteScore
    A
    rok vydaniarok metrikyIFIF Q (best)SJRSJR Q (best)
    202120202.546Q20.699Q2
Počet záznamov: 1  

  Tieto stránky využívajú súbory cookies, ktoré uľahčujú ich prezeranie. Ďalšie informácie o tom ako používame cookies.