Počet záznamov: 1  

Properties of flat-pressed wood-polymer composites made using secondary polyethylene

  1. NázovProperties of flat-pressed wood-polymer composites made using secondary polyethylene
    Aut.údajePavlo Lyutyy...[et al.]
    Preklad názvupodnázvu : Vlastnosti plošne lisovaných drevo-polymérových kompozitov vyrobených zo sekundárnych polyetylénov
    Autor Lyutyy Pavlo
    Spoluautori Bekhta Pavlo
    Sedliačik Ján TUZDFNDV - Katedra nábytku a drevárskych výrobkov
    Ortynska Galina Jevgenivna
    Zdroj.dok. Acta Facultatis Xylologiae Zvolen : vedecký časopis Drevárskej fakulty. Roč. 56, č. 1 (2014), s. 39-50. - Zvolen : Technická univerzita vo Zvolene, 2014
    PoznámkyLit.
    Jazyk dok.angličtina
    KrajinaSlovenská republika
    Systematika539.2/.5
    667.622.5
    678.742.2
    Heslá drevo-polymérové kompozity - wood-polymer composites * mechanické vlastnosti - mechanical properties * fyzikálne vlastnosti - physical properties * plnivá - fillers * polyetylén - polyetylene
    AnotáciaThe influence of wood filler type (particles, flour, mixture of waste chips and sawdust at ratio 10:90), its content (20, 40, and 60 %), board density (800, 900, and 1000 kg×m−3), pressing temperature (160, 180, and 200 °C) and pressing time (6.4, 8.0, and 9.6 min) on the properties of flat-pressed wood-polymer composites (WPC) using a conventional flat-press process was investigated in this study. Dry-blending method was applied for mixing wood fillers and secondary polyethylene (sPE). The highest strength and water resistance were observed in flat-pressed WPC made using wood particles. The highest values of bending strength were noticed in WPC with 40 % content of wood particles and 60 % content of sPE. The further increase or decrease of wood particles content results in reduction of the bending strength values. Water resistance of flat-pressed WPC improves with the increasing of secondary polyethylene contents from 40 % to 80 %. With increasing board density from 800 to 1000 kg×m−3 the properties of flat-pressed WPC also improved. With increasing pressing temperature from 160 to 200 °C and pressing time from 6.4 to 9.6 min the strength of flat-pressed WPC noticeably increased and water resistance considerably improved.
    URLhttps://df.tuzvo.sk/sites/default/files/05-1-14-lyutyy-bekhta-sedliacik-ortynska_1.pdf
    Báza dátxcla - ČLÁNKY
    Druh dok.RBX - rozpis článkov z periodík
    OdkazyPERIODIKÁ-Súborný záznam periodika
    Zväzky2014: 1-2
    článok

    článok

Počet záznamov: 1  

  Tieto stránky využívajú súbory cookies, ktoré uľahčujú ich prezeranie. Ďalšie informácie o tom ako používame cookies.